Paint & Coatings Industry ›› 2016, Vol. 46 ›› Issue (2): 78-82.

Previous Articles     Next Articles

Improvement of Foaming Problem of Environmental Protection Paint Film

Zheng Lvfeng1, Ling Hui 1,2,3, Ning Zhiyong1, Zhang Zhiliang1, Liu Jia1   

  1. 1. Guangdong Sanhe Chemical Technology Co., Ltd., Zhongshan, Guangdong 528429,China; 2. Guangdong Fuhe Industrial Co., Ltd., Zhongshan, Guangdong 528434,China; 3. Guangdong Xinshanhe Development Co., Ltd., Zhongshan, Guangdong 528429, China
  • Online:2016-02-29 Published:2019-06-01

环保型喷漆漆膜起泡问题的改善

郑吕凤1 ,凌 辉1,2,3 ,宁智勇1 ,张志良1 ,刘 家1   

  1. 1、广东三和化工科技有限公司,广东中山 528429;2、广东阜和实业有限公司, 广东中山 528434;3、 广东新山禾发展有限公司,广东中山 528429
  • 作者简介:郑吕凤( 1990—) ,女,助理工程师,主要从事气雾剂产品的研发。

Abstract: In the process of environmental color proofing paint, with LPG according to a certain ratio of material to air jet plate after filling, appear an abnormal phenomenon of film bubbling. lo solve film foaming problem, with LPG application in environmental protection paint as starting point. Through single factor experiment method, study the ratio of materal to gas, paint material viscosity, solvent system, promoter and other factors on the paint blisters. The result show that the nlm foaming phenomenon was improved, while the ratio of material to gas was adjusted to 1. 73: 1, the viscosity of paint was adjusted to 12.5~13.5 s, the amount of true solvent and slow dry solvent was increased. after adding HANSA ADD 1010 auxiliary in the formula, the success of the film bubble is solved.

Key words: environmental protection aerosol paint, propellant, bubbling, ratio of material to gas

摘要: 在环保型喷漆的调色打样过程中,以 LPG(液化石油气)为抛射剂,按一定料气比灌装,喷制样板,出现漆膜起泡的异常现象。 为解决漆膜起泡问题,以 LPG 在环保型喷漆中的应用为切入点,通过单因素实验方法,研究料气比、漆料黏度、溶剂体系、助剂等因素对漆膜起泡的影响。结果表明: 将料气比调整为 1.73 ∶1,涂料黏度调整到 12.5 ~ 13.5 s,增加真溶剂和慢干溶剂用量,漆膜起泡现象有所改善;在配方中添加 HANSA ADD 1010 助剂后,成功解决了漆膜起泡的问题。

关键词: 环保型喷漆, 抛射剂, 起泡, 料气比