Analysis in Blistering of Anticorrosion Coatings for Steel Structure in Grotto Environment

Lou Miao 1,2,Hu Yongle2,Qiang Wenjiang1,Lu Yufeng2,Zhou Meng2   

  1. 1.School of Materials Science and Engueeng, University of Science and Technology Beijing,Beijing 100083, China; 2.Graduate School of Northuest Nuclear Technology, Xi'an 710024, China
  • Online:2010-11-01 Published:2019-05-22

洞室环境钢结构防腐涂层起泡分析

楼 淼1,2,胡永乐2,强文江1,芦玉峰2,周 萌2   

  1. 1. 北京科技大学材料科学与工程学院,北京 100083;2. 西北核技术研究所,西安 710024
  • 作者简介:楼森(1981-),男,硕士,工程师,从事金属材料腐与防护研究。

Abstract: Blistering is one of the most common causes leading to failure of organic coatings. This article has described the micromechanism of the blistering behavior of various organic coatings, analysed the reasons of blistering of corrosion protective coatings on steel structure in grotto environment, and proposed some helpful solutions.

Key words: grotto environment, steel structure, corrosion protection, blistering

摘要: 起泡是有机涂层失效的主要形式之一,介绍了有机涂层起泡失效行为的微观机制,对洞室环境钢结构防腐涂层起泡过程进行了分析,并给出相关建议。

关键词: 洞室环境, 钢结构, 防腐, 起泡