摘要: 常规测定氧化铁颜料中氧化铁含量时产生难以处置完全的含汞废水,污染环境。本文介绍了对有汞测定加以改进的无汞测定法,以甲基橙或三氯化钛代替氯化汞去除残留氯化亚锡。无汞法不仅效果令人满意,而且没有含汞废水,有利于环境保护。
关键词:
氧化铁,
含汞废水,
无汞测定,
甲基橙,
三氯化钛,
环境保护
Abstract: The conventional determination method for iron oxide content in iron oxide pigments will pro-duce a mercury -containing waste water which is difficult to be handled, causing environment pollution.This article has described a new mercury -free determination method for iron oxide, which used methyl or-ange or titanium trichloride instead of mercury chloride for removing of residual SnCL,. This method provided a satisfactory result, and no mercury - contianing waste water discharge.
Key words:
oxide iron,
waste water containing mercury,
mercury -free determination,
methyl orange;titatium trichloride,
environmental protection
凌 浩, 麻 毅. 无汞排放的氧化铁含量测定方法[J]. 涂料工业, 2009, 39(6): 60-61.
Ling Hao, Ma Yi. Determination Method of Iron Oxide Content with No Mercury Discharge[J]. Paint & Coatings Industry, 2009, 39(6): 60-61.