摘要: 【目的】采用自制的封闭型多异氰酸酯固化剂,开发高性能光热太阳能镜背涂料。【方法】以脂肪族六亚甲基二异氰酸酯(HDI)、三羟甲基丙烷(TMP)、3,5-二甲基吡唑为原料合成封闭型多异氰酸酯固化剂。配合功能型聚酯面漆,制备单组分镜背涂料,研究该涂料在光热太阳能镜镜背上的应用性能。【结果】当 n(—NCO)∶n(—OH)为 0. 8∶1时,满足 170 ℃/3 min的快速固化要求。固化后的漆膜铅笔硬度、柔韧性、耐冲击性、耐磨性等优异。耐人工气候老化 4 000 h后漆膜无开裂、粉化,耐 5%中性盐雾 2 000 h后漆膜无边缘腐蚀,漆膜耐温变、耐湿热性能均可达到技术要求。【结论】该光热太阳能镜背涂料性能优异,应用前景广泛。
关键词:
光热太阳能镜,
镜背涂料,
封闭型多异氰酸酯固化剂,
聚酯面漆,
单组分烘烤固化
Abstract: [Objective]To develop a high-performance coatings for the backside of solar thermal mirrors using a self-made blocked polyisocyanate curing agent.[Methods] The blocked polyisocyanate curings agent was synthesized using aliphatic hexamethylene diisocyanate(HDI), trimethylolpropane(TMP),and 3,5-dimethylpyrazole as raw materials. A one-component mirror backcoatings was prepared with functional polyester topcoat,and the application performance of this coatingon the back of solar thermal mirrors was studied.[Results]When the ratio of n(—NCO)to n(—OH) was set at 0.8,the coatings met the requirement of rapid curing at 170 ℃ for 3 minutes. The cured paint film exhibited excellent mechanical properties such as pencil hardness,flexibility,impact resistance and abrasion resistance. After 4 000 h of artificial weathering test,the paint film showed no cracking or chalking. After 2 000 h of 5% neutral salt spray test,the paint film displayed no edgecorrosion. Both of the technical requirements for temperature change resistance and heat and humidityresistance of the paint film were met.[Conclusion] This solar thermal mirror back coating has excellent performance and broad application prospects.
Key words:
solar thermal mirror,
mirror back coatings,
blocked polyisocyanate curing agent,
polyester topcoat,
one-component baking and curing
中图分类号:
汪辉辉, 王李军, 李文凯, 郭亮亮, 周如东, 孔德成, 李 娜. 光热太阳能镜背涂料的制备及应用[J]. 涂料工业, 2026, 56(1): 62-66.
WANG Huihui, WANG Lijun, LI Wenkai, GUO Liangliang, ZHOU Rudong, KONG Decheng, LI Na. Preparation and Application of Back Coatings for Solar Thermal Mirrors[J]. Paint & Coatings Industry, 2026, 56(1): 62-66.